6013 is a light penetrating rod used for sheet metal and thin metal welding.

6010 is a deep penetrating rod. You're supposed use it for open root welds for 100% penetration and then the hot pass.

dustyluce
Автор

The point of doing cap with 7018 is when you use 6010 cellulose rod and low hydrogen cap(7018) prevents cracking in a nutshell. Stay away from 6013 rods, they're shit in most cases and good for welding gates, some minor repairs etc. Slag inclusion is a bastard too.

Mistabushi
Автор

So I’m today years old and I just learned you can throw a root in with a 6013. Friggin welding man

MrDrRemi
Автор

I was always taught to put a root face on the joint so flattening the point of the V…

jackross
Автор

C'est la racine qui est importante dans la démonstration. Dommage que l'on ne puisse la voir !
Il serait bien de faire une démonstration avec l'électrode enrobée basique. Racine en polarité inversée.
Merci

brunoblanc
Автор

We limit 6013 to plates only.. 3/32 at 3 mm gap good choice.. 👍👍

edsantos
Автор

When I first learned how to weld in school. Chasing that key hole was a pain in my ass

indicol
Автор

You could probably just ran 7018 all the way out. Imo it's easier to run then 6013. Plus then it's all 70, 000 tensile strength deposited weld metal.

dustyluce
Автор

why do you need that gap instead of butting the pieces together?Im not a welder I am just curious

eddymack
Автор

How many slag inclusions was in there?

morenothingu
Автор

Ti imas variskra 250amperski inverter ter tudi ac/dc za tig dodatno. Carsko

julijannajger
Автор

Poor rod choice 6010-6011 fast freeze high penetration would have been the preferred choice over a low penetration 6013.. which is usually used on sheet metal 😂😂

joshcormier
Автор

don't mean to be rude but why do people post videos of them welding when thay haven't Learned to weld yet? is it so we can help and give pointers or is it because thay don't know they can't weld yet? I mean I'm not saying its that bad but it's got a ways to go before it's show worthy.

johnscarboroughregenerativ
Автор

Side to side is better not back and forth. You will trap slag in the root pass.

jasonrudy
Автор

Jak ta spoina wygląda na końcach? Ja bym się tym nie chwalił!.

FajnyKtos
Автор

La raíz se debe hacer con electrodos CELULOSICOS TIPO QUEDA MUCHO MEJOR QUE CON RUTILICOS - (TIPO 6013)_además el celulosico (6010), no tiene escoria.... COMO LOS RUTILICOS

jorgealvarofernandezacosta
Автор

Well it looked good for about 3 seconds till it showed the 6013. The fact they are using a 6013 makes me question this whole things legitimacy.
6010 Root with 7018 hot pass. Fill and cap with 7018.

WeldYouLookAtThat
Автор

6010 its beeter for the rooth pass i guess

alejandrormbo
Автор

prep is really nice, ,, the welding is crap.

tomthompson
Автор

60 13 no sirve para soldar, ese calibre de placas, mejor 70 18, buena resistencia y gran penetración,